Open any insert catalog, and before the geometry, before the grade name, and before the price, you will find a colored band with a letter in it. Blue P. Yellow M. Red K. Most people read it as "which metal" and move on. It says more than that, and the part they skip is the number that comes after the letter.
This is the system behind every grade chart you will ever look at, including ours. Five minutes with it saves a lot of trial and error at the machine.
Where the Letters Come From
The groups are defined in ISO 513, the standard that classifies hard cutting materials (carbide, cermet, ceramic, CBN, and diamond) by what they are meant to cut. The original version had only three groups, P, M, and K, sorted by the kind of chip each material makes. Materials kept multiplying, and the current edition splits the work into six main groups.
The letters themselves carry no meaning. Seco Tools puts it plainly: the color is the theoretical color a chip has at the moment it forms when you cut that material. That is a useful way to remember them.
The Six Groups at a Glance
| Group | Color | What it covers | What it does to the edge |
|---|---|---|---|
| P | Blue | Carbon, alloy, and tool steels; cast steel; and the ferritic and martensitic stainless grades | Long chips and heat on the rake face, which shows up as crater wear |
| M | Yellow | Austenitic and duplex stainless steels | Work hardening, built-up edge, and notch wear at the depth-of-cut line |
| K | Red | Gray, ductile (nodular), and malleable cast iron | Short, broken chips and abrasion. Flank wear from the graphite and hard particles. |
| N | Green | Aluminum, copper, brass, and other non-ferrous metals, plus plastics and composites | Material welding to a dull edge. Wants sharp, polished, positive geometry. |
| S | Brown in the standard, orange in most catalogs | Nickel, cobalt, and iron-based superalloys, and titanium | Heat that stays in the edge, work hardening, and notching. The hardest group on tool life. |
| H | Gray | Hardened steel around 45 to 65 HRC, chilled and hardened cast iron | Abrasion and heat at very high cutting pressure |
Two lines in that table cause most of the mistakes.
Not all stainless is M. ISO 513 puts every steel in P except stainless with an austenitic structure. A 304 or a 316 belongs in M. A 410 in the annealed condition behaves much more like an alloy steel and often cuts well with a P grade. If you have been fighting a martensitic stainless with an M grade, that is worth a test.
Titanium is S, not N. It is not iron-based, so people file it next to aluminum. It cuts nothing like aluminum. It holds heat in the edge and work hardens, which is why it shares a group with Inconel.
The Number Is the Part Everyone Skips
After the letter comes a two-digit number: P10, P25, K20, M30. It is called the group of application, and it runs along a single scale.
- Low numbers (01, 05, 10) mean a harder, more wear-resistant grade. It wants a high cutting speed, light feed, and a stable cut. Think finishing.
- High numbers (30, 40, 50) mean a tougher grade that resists chipping. It accepts heavier feeds, interrupted cuts, and less rigid setups at lower speeds. Think roughing.
The trade is always the same one. You cannot have the most wear resistance and the most toughness in the same grade. Moving down the scale buys speed and tool life in a steady cut. Moving up buys survival when the cut hits a keyway, a casting skin, or a long overhang.
The groups do not all run the same length. P goes to 50. M and K stop at 40. N, S, and H stop at 30, because those materials are usually cut under conditions that never call for the toughest end of the scale.
Manufacturers rarely print a single number. A grade is usually shown as a span, for example, P15 to P35 or M20 to M30, and the band on the chart shows where in that span it works best. Seco describes the ranking as rather subjective, and that is honest. The number tells you where a maker positioned its grade against its own range. It is not a lab measurement you can compare across brands to the decimal.
How to Use It at the Machine
Start with the material, then the cut, then the grade.
- Name the group. Look up the alloy, not the color of the bar. If you are not sure, our material pages list it, sorted into families: carbon and alloy steels, stainless and heat-resisting steels, tool and die steels, aluminum alloys, nickel, cobalt and superalloys, titanium alloys, copper, brass and bronze, and cast irons and other alloys.
- Check the hardness. The same 4140 is a P material annealed and an H material after hardening to the high 40s. The hardness conversion chart helps when the print gives Brinell and the catalog speaks Rockwell.
- Describe the cut honestly. Continuous and rigid moves you toward the low numbers. Interrupted, scaled, or on a long overhang moves you up.
- Pick the grade whose span covers that point. If you are at the edge of a span, choose the tougher side first. A grade that wears is a cost. A grade that chips is a scrapped part.
Then read the failure, because it tells you which way to move. Steady flank wear and a long life with no chipping means you have room to go harder, down the scale, and run faster. Chipping, a broken corner or a fractured edge means go tougher, up the scale, before you touch the speed.
What the Letter Does Not Tell You
The group and number describe the grade: its substrate and its coating. They say nothing about the shape of the edge. A K grade on a geometry made for steel will still behave badly in cast iron. The chipbreaker, the edge hone, and the rake angle are chosen separately, which is why the insert designation and the grade name are two different parts of the order.
It also does not replace cutting data. It narrows the choice. The machining data chart gives you a starting point for speed and feed once the grade is picked.
Going Deeper
We have written about pieces of this before, and this article is the map that ties them together.
- Understanding the Application Range of Cutting Tools walks through the numbered scale in more detail.
- What Is Machinability of Materials explains why one alloy cuts easily and its neighbor does not.
- Machining Stainless Steel: One Mechanism Explains Almost Every Problem is the companion piece for the M group.
- Machinability of Titanium and Machinability of Heat-Resistant Superalloys cover the S group in depth.
- A Simple Guide to Substrate Carbide Grades explains what sits under the coating.
- Reading the chip covers what chip shape and color tell you before the tool fails.
- Ceramic Turning Inserts covers the point where carbide stops being the right answer in K, S, and H work.
When you have the group and the cut, our carbide grades guide and grade look-up show where each grade sits, and the turning inserts are sorted so you can filter to it. Not sure where your job falls? Call +1 223-227-2433 (223-CARBIDE) with the material, the hardness, and how the part is held, and we will point you to a grade.
Frequently Asked Questions
What does P25 mean on an insert?
P is the material group, steel. 25 is the position on the wear-resistance-to-toughness scale: a middle grade suited to general turning of steel at moderate speed and feed. Lower numbers such as P10 are harder and faster for finishing. Higher numbers such as P40 are tougher for roughing and interrupted cuts.
Is a lower ISO number better?
No. It is harder and more wear-resistant, which is better in a stable, continuous cut. In an interrupted or unstable cut, the same grade is more likely to chip. The right number depends on the cut, not on a ranking.
Which ISO group is stainless steel?
Austenitic and duplex stainless, such as 304, 316, and 2205, are group M. ISO 513 places the other stainless types with steels in group P, and martensitic grades in the annealed condition often cut well with a P grade.
Is titanium in group N with aluminum?
No. Titanium alloys are group S, together with nickel and cobalt superalloys. They hold heat in the cutting edge and work harden, which is the opposite of how aluminum behaves.
Can I compare P20 from two different brands directly?
Only roughly. Each manufacturer positions its own grades on the scale, and the ranking is partly a judgment call. Use the numbers to compare grades within one brand, and treat a cross-brand match as a starting point to test.