Ferrium® S53®
In short: Ferrium S53 is a corrosion-resistant, ultra high-strength steel developed for structural aerospace. It delivers mechanical properties equal to or better than conventional ultra high-strength steels such as 300M and SAE 4340, with the added benefit of resistance to corrosion and to stress-corrosion cracking. Equivalents: AMS 5922, UNS S10500. As starting points, turn it at Not published by the mill m/min (See note SFM) and mill it at 69 – 79 m/min (225 – 260 SFM). FM Carbide recommends for turning, grade FM2553 (CVD, M30); for milling, FM125 (PVD, M15 – M35).
Material Overview
Ferrium S53 is a corrosion-resistant, ultra high-strength steel developed for structural aerospace. It delivers mechanical properties equal to or better than conventional ultra high-strength steels such as 300M and SAE 4340, with the added benefit of resistance to corrosion and to stress-corrosion cracking. The alloy is strengthened by an efficient M2C dispersion precipitated during tempering while other carbides are avoided, which is what lets it hold strength, wear resistance, and toughness at the same time. A passive oxide film gives it corrosion resistance comparable to 440C stainless.
Its high hardenability permits less severe quench conditions and therefore less distortion in heat treatment. A practical advantage on the large, expensive parts it is specified for: landing gear, actuators, drive shafts, structural members, and fasteners. Ferrium S53 is manufactured and sold by Carpenter Technology under license from QuesTek Innovations LLC and is covered by U.S. Patent 7,967,927 B2.
International Designation Equivalents
| Standard | Designation |
|---|---|
| AMS | 5922 |
| UNS | S10500 |
Ferrium S53 is a proprietary alloy, so it has no DIN, EN, or JIS equivalent. The AMS and UNS numbers above are the only recognized designations.
Chemical Composition
| Element | Nominal content |
|---|---|
| Iron (Fe) | Balance |
| Cobalt (Co) | 14.00% |
| Chromium (Cr) | 10.00% |
| Nickel (Ni) | 5.50% |
| Molybdenum (Mo) | 2.00% |
| Tungsten (W) | 1.00% |
| Vanadium (V) | 0.30% |
| Carbon (C) | 0.21% |
Single figures are nominal. The composition previously published on this page omitted vanadium and listed phosphorus and sulfur limits that the mill does not publish; the table above is the type analysis from Carpenter Technology's own datasheet.
Machinability Explained
The decision that matters on Ferrium S53 is when you cut it, not how fast. In the annealed condition the alloy machines are about like 300M at 35 HRC, and Carpenter states plainly that the tools used for cutting and drilling are typically those used for other 400 series stainless steels. That is the window where the bulk of the material should come off. Anneal is 1255°F (680°C) for 8 hours, air cooled, which brings the stock to 327 HB or lower.
After solution treatment, cold treatment, and the double temper, the part sits near 54 HRC with a tensile strength around 288 ksi: at that point it is an ultra-high-strength steel, and the annealed speeds no longer apply. Two details decide whether the finished part comes out to print: heat-treat growth is typically uniform at roughly 0.002–0.003 in. per inch, so leave stock for it, and the alloy is subject to decarburization during hardening, so heat treatment should take place in a neutral atmosphere furnace, salt bath, or vacuum. If a preheat is used, keep it no higher than 600°F (315°C).
Recommended Cutting Speeds
| Operation | Vc (m/min) | Vc (SFM) | Condition |
|---|---|---|---|
| Milling | 69 – 79 | 225 – 260 | Annealed, ~35 HRC |
| Drilling | 76 – 91 | 250 – 300 | Annealed, ~35 HRC |
| Turning | Not published by the mill | See note | |
The milling and drilling figures are Carpenter's published recommendations and apply to annealed material at about 35 HRC. Carpenter publishes no turning speed for S53; start from our guidance for 400 series martensitic stainless and verify with a test cut. For hardened material near 54 HRC, treat the job as hard steel turning: speeds fall substantially and CBN or ceramic should be considered where volume justifies it.
Recommended FM Carbide Grades
Turning
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM2553 | CVD | M30 |
| FM324 | PVD | M10 – M20 |
Parting / Grooving
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM2553 | CVD | M30 |
| FM2543 | CVD | P20 |
Milling
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM125 | PVD | M15 – M35 |
These are the grades we recommend for 400 series martensitic stainless, which is the tooling family the mill points to for annealed S53. They are a starting point, not a published S53 recommendation. Machining the alloy in the hardened condition is a different job. Send us the hardness and the operation and we will match it.
Typical Mechanical Properties
| Property | Value |
|---|---|
| Tensile strength | 288 ksi / 1986 MPa |
| Yield strength | 225 ksi / 1551 MPa |
| Elongation in 4D | 15% |
| Reduction of area | 55 – 57% |
| Fracture toughness | 65 ksi√in / 71 MPa√m |
| Density | 0.2880 lb/in³ |
| Elastic modulus (E) | 29.6 × 10³ ksi |
Room-temperature values in the heat-treated condition, longitudinal and transverse.
Heat Treatment Reference
| Step | Schedule |
|---|---|
| Normalizing | 1975°F (1080°C) for 1 hour, air cool |
| Annealing | 1255°F (680°C) for 8 hours, air cool: 327 HB or lower |
| Solution treatment | 1985°F (1085°C) for 1 hour, oil quench, or equivalent |
| Cold treatment | −100°F (−73°C) for 1 hour, air warm |
| Tempering | 934°F (501°C) for 3 hours and quench, then −100°F for 1 hour, then 900°F (482°C) for 12 hours, air cool |
Included because the machining sequence depends on it. Confirm the schedule against the mill datasheet and your own specification before processing parts.
Ferrium® S53® questions
What is Ferrium® S53®?
Ferrium S53 is a corrosion-resistant, ultra high-strength steel developed for structural aerospace. It delivers mechanical properties equal to or better than conventional ultra high-strength steels such as 300M and SAE 4340, with the added benefit of resistance to corrosion and to stress-corrosion cracking.
What is the equivalent of Ferrium® S53®?
AMS 5922, UNS S10500.
What is the chemical composition of Ferrium® S53®?
Iron (Fe) Balance, Cobalt (Co) 14.00%, Chromium (Cr) 10.00%, Nickel (Ni) 5.50%, Molybdenum (Mo) 2.00%, Tungsten (W) 1.00%, Vanadium (V) 0.30%, Carbon (C) 0.21%.
What cutting speed should I use for Ferrium® S53®?
Starting points: milling 69 – 79 m/min (225 – 260 SFM), drilling 76 – 91 m/min (250 – 300 SFM), turning Not published by the mill m/min (See note SFM). Adjust for machine rigidity, workholding and tool condition, and use the Speeds & Feeds Calculators for RPM and feed.