Ti-5Al-2.5Fe (Tikrutan)
In short: Ti-5Al-2.5Fe is an alpha-beta titanium alloy created as a vanadium-free alternative to Ti-6Al-4V for surgical implants. The idea is simple: keep the two-phase structure that gives Ti-6Al-4V its strength, but use iron instead of vanadium as the beta stabilizer. Equivalents: ISO 5832-10, Trade name Tikrutan. As starting points, turn it at 70 – 90 m/min (230 – 300 SFM) and mill it at 50 – 70 m/min (160 – 230 SFM). FM Carbide recommends for turning, grade FM524 (CVD, S05 – S10); for milling, FM125 (PVD, S15 – S35).
Material Overview
Ti-5Al-2.5Fe is an alpha-beta titanium alloy created as a vanadium-free alternative to Ti-6Al-4V for surgical implants. The idea is simple: keep the two-phase structure that gives Ti-6Al-4V its strength, but use iron instead of vanadium as the beta stabilizer. It is covered by ISO 5832-10, the implant-materials standard for wrought titanium 5-aluminium 2.5-iron alloy, and it is supplied under the Tikrutan trade name. Published cytocompatibility work found it as cytocompatible as Ti-6Al-4V under the same surface treatments (Bordji et al., 1996).
In the shop it behaves like what it is: an alpha-beta titanium in the same strength class as Grade 5. If you have cut Ti-6Al-4V, you already know this material: the approach, the speeds, and the failure modes are the same. Because most of what is made from it ends up as an implant, surface integrity and contamination control usually matter more on these parts than cycle time does.
International Designation Equivalents
| Standard | Designation |
|---|---|
| ISO | 5832-10 |
| Trade name | Tikrutan |
This is a specialty implant alloy, so it has no AISI or UNS number in general industrial use the way Ti-6Al-4V (R56400) does.
Chemical Composition
| Element | Nominal content |
|---|---|
| Titanium (Ti) | Balance |
| Aluminum (Al) | ~5% |
| Iron (Fe) | ~2.5% |
| Vanadium (V) | None: iron replaces it |
Nominal values, which is what the alloy name states. ISO 5832-10 sets the full ranges, including the interstitial limits for oxygen, nitrogen, carbon, and hydrogen that govern implant material. Consult the standard or the mill certificate for the limits that apply to your lot. The previous version of this page published no composition at all.
Machinability Explained
Every difficulty of machining titanium applies here. Thermal conductivity is roughly a sixth that of steel, so cutting heat stays at the tool tip instead of leaving with the chip, and titanium's chemical reactivity with tool materials at those temperatures drives diffusion wear and cratering. That is why titanium speeds run a fraction of steel speeds: it is a heat problem, not a strength problem.
The low modulus of elasticity is the second half of it: titanium deflects under cutting pressure more than steel does at the same force, so a setup that would be rigid enough for steel will chatter, push off, and rub. And rubbing is the thing to avoid above all, because the alloy work-hardens the instant a tool stops shearing. The fundamentals are the familiar ones: keep speeds low, keep feeds high enough to stay under any hardened layer from the previous pass, make the setup as rigid as you can, and flood the cut with coolant. Sharp tooling and modest tool-life expectations come with the territory.
Recommended Cutting Speeds
| Operation | Vc (m/min) | Vc (SFM) |
|---|---|---|
| Turning | 70 – 90 | 230 – 300 |
| Milling | 50 – 70 | 160 – 230 |
| Parting | 45 – 60 | 150 – 200 |
| Grooving | 60 – 80 | 200 – 260 |
| Drilling | 60 – 80 | 200 – 260 |
These are the starting points we publish for Ti-6Al-4V, the alpha-beta titanium this alloy was designed to replace and the closest material we have verified data for. They are not an ISO 5832-10 recommendation. Values assume a well-matched insert grade, maximum rigidity, good-quality stock, short overhang, and flood coolant; reduce further for interrupted cuts, thin walls, or anything less than a rigid setup.
Recommended FM Carbide Grades by Operation
Turning
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM524 | CVD | S05 – S10 |
| FM2533 | CVD | S15 |
Parting Off
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM2543 | CVD | S20 |
| FM2553 | CVD | S30 |
Grooving
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM2533 | CVD | S10 |
Milling (Indexable)
| Grade | Coating | ISO Application Range |
|---|---|---|
| FM125 | PVD | S15 – S35 |
Recommended Insert Cutting-Edge Geometry
| Parameter | Value |
|---|---|
| Honing Size | 0.02 – 0.05 mm / 0.001 – 0.002" |
| Rake Angle | 13° – 18° |
| Land Angle | Neutral |
| Land Width | 0.10 – 0.20 mm / 0.004 – 0.008" |
| Ground Insert | Recommended |
Ti-5Al-2.5Fe (Tikrutan) questions
What is Ti-5Al-2.5Fe (Tikrutan)?
Ti-5Al-2.5Fe is an alpha-beta titanium alloy created as a vanadium-free alternative to Ti-6Al-4V for surgical implants. The idea is simple: keep the two-phase structure that gives Ti-6Al-4V its strength, but use iron instead of vanadium as the beta stabilizer.
What is the equivalent of Ti-5Al-2.5Fe (Tikrutan)?
ISO 5832-10, Trade name Tikrutan.
What is the chemical composition of Ti-5Al-2.5Fe (Tikrutan)?
Titanium (Ti) Balance, Aluminum (Al) ~5%, Iron (Fe) ~2.5%, Vanadium (V) None: iron replaces it.
What cutting speed should I use for Ti-5Al-2.5Fe (Tikrutan)?
Starting points: turning 70 – 90 m/min (230 – 300 SFM), milling 50 – 70 m/min (160 – 230 SFM), parting 45 – 60 m/min (150 – 200 SFM), grooving 60 – 80 m/min (200 – 260 SFM), drilling 60 – 80 m/min (200 – 260 SFM). Adjust for machine rigidity, workholding and tool condition, and use the Speeds & Feeds Calculators for RPM and feed.