Technical Reference Library

ASTM A479 Stainless Steel Bar

ASTM A479 / ASME SA-479Product Bars and shapesUse Boilers and pressure vessels

In short: ASTM A479 is not a single alloy. It is the specification for stainless steel bars and shapes used in boilers and other pressure vessels: rounds, squares, hexagons, angles, tees and channels, hot or cold finished. It covers austenitic, duplex (austenitic-ferritic), ferritic and martensitic grades, so the machining behavior depends on the grade stamped next to "A479" on the cert, for example 316/316L or 2507.

What A479 covers

A479 covers hot- and cold-finished stainless bars, including rounds, squares and hexagons, plus hot-rolled or extruded shapes such as angles, tees and channels, for boiler and pressure vessel construction. Four families of stainless are included: austenitic, austenitic-ferritic (duplex), ferritic and martensitic. Austenitic grades must be heat treated and are subject to a corrosion test.

In the shop, "A479" on a bar tells you it was produced for pressure service. To pick tools and speeds, look at the grade.

Common grades bought to A479

Grade UNS Family Machining data
304 / 304L S30400 / S30403 Austenitic Steel 304, 304L
316 / 316L S31600 / S31603 Austenitic Steel 316, 316L
2507 super duplex S32750 Duplex Super duplex 2507

Grade examples from Rolled Alloys (316/316L) and Alleima (2507) data sheets that list ASTM A479 among their product standards.

Machining A479 bar

Machine A479 material according to its grade. Austenitic bars (304, 316) work harden, so keep the edge sharp and the feed steady and never let the tool dwell. Duplex and super duplex bars are much stronger, with 80 ksi minimum yield for 2507, and need lower cutting speeds and a tough, heat-resistant grade. The linked grade pages give starting speeds and insert grades.

ASTM A479 Stainless Steel Bar questions

What is ASTM A479?

ASTM A479/A479M is the standard specification for stainless steel bars and shapes for use in boilers and other pressure vessels. It covers austenitic, duplex, ferritic and martensitic grades in hot- and cold-finished form.

What is the difference between ASTM A276 and A479?

A276 is the general specification for stainless steel bars and shapes. A479 is written for boiler and pressure vessel use and adds requirements such as heat treatment and corrosion testing of the austenitic grades. Pressure equipment codes reference A479 (ASME SA-479).

Is A479 316L the same as 316L?

Yes in chemistry: A479 316L is UNS S31603. The A479 designation adds the product form and the testing requirements of that specification. See our 316L page for machining data.

Which grades are available under A479?

Austenitic grades such as 304/304L and 316/316L, duplex grades including 2507 (S32750), plus ferritic and martensitic grades.

Get tooling tips by email

New TechTips, TechTalks and tool releases. No spam.